Segui
Sufyan Garoushi
Sufyan Garoushi
Email verificata su utu.fi - Home page
Titolo
Citata da
Citata da
Anno
Physical properties and depth of cure of a new short fiber reinforced composite
S Garoushi, E Säilynoja, PK Vallittu, L Lassila
Dental Materials 29 (8), 835-841, 2013
3872013
Short glass fiber reinforced restorative composite resin with semi-inter penetrating polymer network matrix
S Garoushi, PK Vallittu, LVJ Lassila
Dental materials 23 (11), 1356-1362, 2007
2442007
Influence of increment thickness on light transmission, degree of conversion and micro hardness of bulk fill composites
S Garoushi, P Vallittu, A Shinya, L Lassila
Odontology 104, 291-297, 2016
1482016
Characterization of fluoride releasing restorative dental materials
S Garoushi, PK Vallittu, L Lassila
Dental Materials Journal 37 (2), 293-300, 2018
1462018
Translucency of flowable bulk-filling composites of various thicknesses
LVJ Lassila, E Nagas, PK Vallittu, S Garoushi
Chinese journal of dental research 15 (1), 31, 2012
1452012
Static and fatigue compression test for particulate filler composite resin with fiber-reinforced composite substructure
S Garoushi, LVJ Lassila, A Tezvergil, PK Vallittu
dental materials 23 (1), 17-23, 2007
1412007
Load bearing capacity of fibre-reinforced and particulate filler composite resin combination
S Garoushi, LVJ Lassila, A Tezvergil, PK Vallittu
Journal of dentistry 34 (3), 179-184, 2006
1342006
Polymerization shrinkage of experimental short glass fiber-reinforced composite with semi-inter penetrating polymer network matrix
S Garoushi, PK Vallittu, DC Watts, LVJ Lassila
Dental Materials 24 (2), 211-215, 2008
1302008
Short fiber‐reinforced composite restorations: a review of the current literature
S Garoushi, A Gargoum, PK Vallittu, L Lassila
Journal of investigative and clinical dentistry 9 (3), e12330, 2018
1242018
Mechanical and structural characterization of discontinuous fiber-reinforced dental resin composite
J Bijelic-Donova, S Garoushi, LVJ Lassila, F Keulemans, PK Vallittu
Journal of dentistry 52, 70-78, 2016
1152016
Influence of staining solutions and whitening procedures on discoloration of hybrid composite resins
S Garoushi, L Lassila, M Hatem, M Shembesh, L Baady, Z Salim, ...
Acta Odontologica Scandinavica 71 (1), 144-150, 2013
1072013
Mechanical properties and fracture behavior of flowable fiber reinforced composite restorations
L Lassila, F Keulemans, E Säilynoja, PK Vallittu, S Garoushi
Dental Materials 34 (4), 598-606, 2018
1062018
Oxygen inhibition layer of composite resins: effects of layer thickness and surface layer treatment on the interlayer bond strength
J Bijelic‐Donova, S Garoushi, LVJ Lassila, PK Vallittu
European journal of oral sciences 123 (1), 53-60, 2015
1052015
Mechanical properties, fracture resistance, and fatigue limits of short fiber reinforced dental composite resin
J Bijelic-Donova, S Garoushi, PK Vallittu, LVJ Lassila
The Journal of prosthetic dentistry 115 (1), 95-102, 2016
1042016
Short fiber reinforced composite: the effect of fiber length and volume fraction
SK Garoushi, LV Lassila, PK Vallittu
J Contemp Dent Pract 7 (5), 10-17, 2006
952006
Preliminary clinical evaluation of short fiber-reinforced composite resin in posterior teeth: 12-months report
S Garoushi, J Tanner, PK Vallittu, L Lassila
The open dentistry journal 6, 41, 2012
892012
Direct restoration of severely damaged incisors using short fiber-reinforced composite resin
S Garoushi, PK Vallittu, LVJ Lassila
Journal of dentistry 35 (9), 731-736, 2007
872007
The effect of short fiber composite base on microleakage and load-bearing capacity of posterior restorations
SK Garoushi, M Hatem, LVJ Lassila, PK Vallittu
Acta biomaterialia odontologica Scandinavica 1 (1), 6-12, 2015
792015
Short fiber reinforced composite: a new alternative for direct onlay restorations
S Garoushi, E Mangoush, M Vallittu, L Lassila
The open dentistry journal 7, 181, 2013
772013
Fracture resistance of short, randomly oriented, glass fiber-reinforced composite premolar crowns
S Garoushi, PK Vallittu, LVJ Lassila
Acta biomaterialia 3 (5), 779-784, 2007
742007
Il sistema al momento non può eseguire l'operazione. Riprova più tardi.
Articoli 1–20